Cs0.32WO3 for thermal insulation coating can be synthesized by hydrothermal method using sodium tungstate and cesium carbonate as raw materials. Wherein, cesium carbonate was added to the tungstic acid solution obtained by ion exchange of sodium tungstate according to Cs/W ratios of 0.1, 0.2, 0.3, 0.4, 0.5, and 0.6, respectively. More details, please visit: http://cesium-tungsten-bronze.com/index.html According to the experts, the near-infrared shielding performance of the obtained Cs0.32WO3 nano powder changed with the Cs/W ratio of the raw material, which was…