Blue tungsten oxide for infrared absorption material may be added to tungsten powder, and therefore be applied for sintering tungsten skeleton. 11.22μm of blue tungsten oxide powder with a mass fraction of 5%, 10%, and 15% was added to 2μm of tungsten powder, respectively. And the mixing powder was performed reduction sintering at 1300~1500°C. How does the density of the obtained tungsten skeleton change? Under the same molding pressure, the density of the skeleton compacts with different blue tungsten oxide…